Menene Sashen Baturi?
"Daki"yana nufin tsarin tsari a cikin fakitin baturi wanda ke riƙe da tsara sel. Yana da sauƙi, amma ainihin ma'anar wannan kalma ya bambanta sosai daga kamfani zuwa kamfani. Lokacin da nake a Rivian, kowa ya kira shi "mai ɗaukar kwayar halitta." Bayan na ƙaura zuwa mai siyar da Tier-1 na Koriya, duk takaddun ciki suna magana da shi a matsayin "gidaje na zamani." Abu ɗaya, suna daban.
Na kasance a cikin wannan masana'antar har tsawon shekaru 11, kuma tabbas na shafe lokaci mai yawa akan ƙirar ɗaki fiye da kowane tsarin ƙasa. Ba don fasahar kanta tana da wahala musamman; saboda an haɗe shi da kusan komai. Canja girma ɗaya na ɗakin, kuma dole ne ku sake{3}} sarrafa thermal, structural, and the meetings all over.

Bari in mayar da hankali kan karfin kumburin tantanin halitta - anan ne na shiga cikin mafi yawan ramummuka.
Kowa ya san ƙwayoyin prismatic suna kumbura yayin zagayowar caji/fitowa, amma nawa a zahiri suke kumbura ya bambanta sosai dangane da bayanan mai kaya. Na ga takaddun bayanan CATL suna da'awar kumburin 8% na rayuwa don ƙarfin da aka bayar, yayin da Samsung SDI ya lissafa 12% don kwatankwacin tantanin halitta. Lokacin da ka tambayi injiniyoyinsu, suna cewa "Sharuɗɗan gwaji daban-daban." Wanne ne daidai? Babu wanda ya sani da gaske. Don haka a cikin ƙira, koyaushe muna ɗaukar mafi muni{6}} ƙimar shari'a (12%) sannan mu yi amfani da wani yanayin aminci na 1.2×.
A cikin 2021, na yi aiki a kan wani aiki don OEM OEM (ba zan iya kiran su ba). Ƙarfe na ƙarshen ɗakin sun kasance 2.5 mm hatimi karfe. Mun gudanar da ɗimbin gyare-gyare na CAE - damuwa da nakasar duk sunyi kyau. Bayan haka, kimanin watanni 14 bayan SOP, gazawar filin ta fara birgima. Lokacin da muka yayyaga fakitin, faranti na ƙarshe sun sunkuyar da kai waje. Girgizar ta bayyana tsakanin mai cike da rata da farantin sanyi, juriya na zafi ya tashi, kuma wasu sel suna gudana digiri 7-8 fiye da maƙwabtansu. BMS bai jefa laifi ba saboda bai kai gaci ba tukuna, amma haɓakar tsufa ya zama makawa. A ƙarshe mun canza zuwa 4 mm mutu{16}} jefar da ƙarshen aluminum kuma batun ya ɓace.(Ba zan ambaci nawa wannan lissafin sake aikin ya duba ba.)

Me yasa simulation bai kama shi ba?
Saboda kumburi -harkar lodin ƙarfi da muka ciyar a CAE ba daidai ba ne. An auna bayanan masana'anta tantanin halitta a madaidaicin digiri 25. A zahiri, lokacin da motar ke tafiya a kusa da Phoenix a lokacin rani, shirya yanayin zafi akai-akai ya wuce digiri 45. Fadada yanayin zafi na Electrolyte + haɓakar haɓakar SEI=ƙarfin kumburi na ainihi sama da ƙimar bayanan bayanai. Babu wanda ya san ainihin mai yawa. Bayan wannan bala'i, Ban taɓa amincewa da simulation shi kaɗai ba - yanzu mun ba da umarnin tabbatar da ingancin hawan keke mai zafi a kowane sabon ƙira.
Kwayoyin Silindrical labari ne mabanbanta.
Domin 21700s ko 4680s, mafi yawan taurin radial suna fitowa daga gwangwani da kanta; fadada axial karami ne. Babban damuwa shine tazara da hanyar gyarawa.
Fakitin tsari na Tesla na 4680 hanya ce mai ban sha'awa: sel suna haɗe kai tsaye tare da manne ga manyan zanen gado na sama da na ƙasa, yadda ya kamata suna juya sel cikin nauyi{1}}mambobi.
Babban fa'ida:kawar da nauyin ɗaki na gargajiya.
Babban fage:rashin sabis ɗin sifili - ɗayan mugun tantanin halitta kuma gabaɗayan fakitin guntu ne.
Da kaina, Ina tsammanin wannan ciniki{0}kashe yana da cikakkiyar ma'ana ga ƙirar kasuwancin Tesla (haɗin kai tsaye + tunanin gigacasting), amma bai dace da kowane OEM wanda ke ba da fifikon sabis ba. Injiniyoyin Ford da GM da na yi magana da su har yanzu suna nace akan na'urori masu cirewa.
Hannun cylindrical gama gari{0}}hanyoyin gyara tantanin halitta:
Bakin filastik tare da karyewa{0}} daidai: mafi arha, mafi kyau ga babban taro -, amma kula da rarrafe - PA66 GF30 zai lalace a ƙarƙashin nauyin nauyi sama da digiri 50.
Ƙare -ƙulla faranti: gaba dayan jeren ana matse shi tsakanin faranti masu tarawa a ƙarshen duka.
Haɗin haɗin gwiwa: daidai abin da Tesla yake yi.

Bonding yana da kunkuntar tsari taga.
Ƙananan mannewa → rashin isasshen ƙarfin haɗin gwiwa.
Yayi yawa → ambaliya akan bangon tantanin halitta, yana cutar da canjin zafi.
Maganin lokaci wani ciwon kai ne. A kan aikin ɗaya mun yi amfani da mannen tsari na Henkel (Gano wani abu, ba za a iya tuna ainihin sa ba) wanda ya ƙayyade 24 h a zafin jiki, amma layinmu ya ba da izinin zama na sa'o'i 4 kawai. Mun ƙare zuwa canzawa zuwa 60 digiri / 2 h zafi{{6} taimako magani, wanda ke nufin ƙara dukan tashar dumama da kuma sake yin shimfidar layi.
Bayani mai sauri akan kaurin kushin thermal(wannan ana tambaya da yawa):
- 0.5 mm padyawanci yakan fita a 3-5 W/m·K.
- 1.0 mm padyana buɗe sama mafi girma{0}zaɓuɓɓukan ɗabi'a (wasu sun kai 6-8 W/m·K), amma jimlar juriyar zafi ba koyaushe mafi kyau ba saboda ƙarin kauri.
Dole ne ku gudanar da lambobi don kowane harka. Mafi kauri suna ɗaukar ƙarin juzu'i{1} sama (waɗanda ke yin tantanin halitta da masu yin fakiti duka suna ƙauna), amma aikin zafi na ƙarshe dole ne a inganta shi da kayan aiki na gaske.
Game da dakunan sanyaya nutsewa- Ba ni da hannuwa da yawa{1} akan gogewa, don haka ba zan yi hasashe ba. Abin da na sani shi ne cewa buƙatun rufewa suna da muni (IP67 ko ma IP68), kuma dacewa da kayan aiki tare da ruwan dielectric yana da mahimmanci - wasu robobi suna laushi ko kumbura lokacin da aka jiƙa. Motsi na XING a Taiwan ya yi ayyukan nutsewa da yawa; Fararen takardunsu cikakkun bayanai ne kuma sun cancanci karantawa idan kuna sha'awar.