Babban ra'ayin shine kai tsaye - ka saka siraren siraren carbon akan kayan baturi don sa su zama masu aiki. LFP ba tare da murfin carbon yana da haɓakawa a kusa da 10 ^ -9 S / cm wanda shine ainihin insulator. Ƙara 2-3 wt% carbon shafi kuma kuna samun 10^-3 S/cm, isa ya yi baturi mai aiki.

Muna gudanar da tsarin CVD biyu da layukan suturar sinadarai a wurin mu. CVD yana ba da mafi kyawun daidaituwa amma farashi mai yawa. Rufin rigar yana aiki lafiya don yawancin aikace-aikace kuma kayan aiki sun fi sauƙi.
Duba iyawar murfin CVD don ƙarin cikakkun bayanai akan babban zaɓi na ƙarshe{{0}.
Me yasa Kayayyakin Sufa da Carbon?
Yawancin phosphate - tushen cathodes suna buƙatar shi. Ƙarfin lantarki yana da muni ba tare da sutura ba. Iron phosphate, manganese phosphate - labari iri daya. Ko da wasu oxide cathodes suna amfana daga sutura idan kuna tura manyan ƙimar C-.
Har ila yau, murfin yana aiki azaman kariya mai kariya tsakanin cathode da electrolyte. Wannan yana da mahimmanci a yanayin zafi mai tsayi inda halayen gefe suka hanzarta. Mun ga rayuwar sake zagayowar ta inganta 40-50% kawai daga shafi, musamman lokacin da sel ke gudana sama da digiri 45.
Silicon anodes dabba ce daban. Ƙarar girma yayin hawan keke (300-400%) zai fashe mafi yawan sutura. Kuna buƙatar sassauƙan tsarin carbon ko rufin ya gaza bayan ƴan hawan keke. Mun yi aiki a kan wannan matsala na tsawon shekaru uku kafin mu sami wani tsari wanda a zahiri ya yi hawan keke 200 da suka wuce.
Tsarin Rufe CVD
Saitin CVD ɗin mu yana amfani da acetylene ko methane gas a 650{2}}750 digiri . Matsakaicin kwarara ya dogara da girman batch - yawanci 50-200 sccm don nau'in kilogiram 100. Gas din yana rubewa a saman barbashi kuma ya samar da Layer carbon.
Ikon kauri shine ta lokaci da zafin jiki na mintuna a digiri 700 yana samun kusan 5-8 nm dangane da ma'auni. Idan kuna buƙatar sutura mai kauri kuna gudu ta tsawon lokaci, amma kula da toshe pore musamman tare da kayan yanki mai tsayi.
Abubuwan da ke cikin hoto na CVD carbon ya fi rigar hanyoyin sinadarai, wanda ke nufin mafi kyawun aiki. Acetylene yana ba da carbon mai hoto fiye da methane amma kuma ya fi tsada da nau'in zafi don ɗaukar lafiya.
Girman batch akan layin CVD ɗin mu yana daga 10 kg zuwa 200 kg. Manyan batches suna yiwuwa amma daidaituwar yanayin zafi ya zama matsala. Mun koyi wannan ta hanya mai wahala - gudanar da bacin kilogiram 500 sau ɗaya kuma abin da ke kan kayan daga tsakiya da gefuna ya bambanta sosai.
Hanyar Sinadari Rigar
Mix foda tare da maganin glucose, bushe shi, sannan pyrolyze a cikin yanayin nitrogen. A sugar carbonizes kuma suturta barbashi. Hankali mai sauƙi amma samun sa uniform yana ɗaukar ɗan gwaji da kuskure.
pH na maganin glucose yana da mahimmanci. Don kayan yau da kullun kamar LFP muna kiyaye pH a kusa da 4{3}} 5 don haka glucose ya fi dacewa. Matakin bushewa yana da mahimmanci - idan kun bushe da sauri za ku gaji. Muna amfani da bushewar feshi a yanzu wanda ke aiki da kyau fiye da saitin na'urar busar da tsohuwar mu.
Yawan zafin jiki na Pyrolysis shine digiri 500-650 don glucose. Mafi girman yanayin zafi yana ba da ƙarin ƙirar carbon amma kuna fara ƙona yawan amfanin carbon. Citric acid wani zaɓi ne, yana ba da sakamako iri ɗaya ga glucose. Wasu abokan ciniki sun fi son sucrose amma a gaskiya ba mu ga bambancin aiki da yawa ba.
Carbon daga rigar rufi yawanci amorphous ne tare da wasu gajerun wuraren zane-zane{0}. Haɓakawa yana da kyau, baya da kyau kamar CVD amma yana da kyau ga yawancin batura. Kudin yana da kusan 40% ƙasa da CVD kowace kilogiram na kayan da aka rufe.
Aikace-aikace Munyi Aiki Akan
LFP cathodes tabbas 70% na ƙarar murfin mu. Daidaitaccen ƙayyadaddun bayanai shine 2.5 wt% carbon, 8-10 nm kauri. Wasu abokan ciniki suna son 3% don aikace-aikacen ƙimar mafi girma.
Hakanan muna sutura LTO anodes, kodayake ƙasa da yawa. Yawanci 1-1.5 wt% carbon ya isa tun lokacin da aikin LTO ba shi da kyau kamar LFP. Rufin yana taimakawa tare da babban ƙarfin caji wanda ke da mahimmanci don aikace-aikacen caji mai sauri.
NCM811 da sauran nickel{1} arziƙin cathodes wani lokaci ana lulluɓe don kwanciyar hankali maimakon aiki. Kaurin murfin ya fi sirara, watakila 3{5}}5nm, kawai ya isa ya rage hulɗa kai tsaye tsakanin cathode da electrolyte. Wannan yana rage rushewar ƙarfe na miƙa mulki wanda shine yanayin gazawa don kayan arziƙin nickel a babban ƙarfin lantarki.
Silicon composite anodes suna da kalubale. Daidaitaccen sutura ba ya aiki saboda batun faɗaɗa ƙara. Mun ƙirƙira ƙirar murfin carbon tare da ɗan elasticity ta amfani da polymer{2}} carbon da aka samu. Yana da tsada amma ita ce kawai hanyar da muka samu don samun rayuwa mai kyau. Ko da a lokacin, kana kallon watakila 500-800 zagayowar kafin gagarumin iya aiki Fade.
Wani kamfani na kera motoci ya so mu sa kayan gwajin su na manganese{0}} wadataccen kayan cathode. Wannan aikin bai yi aiki ba - kayan ba su da ƙarfi a cikin sinadarai yayin aikin shafa kuma mun ci gaba da ganin canje-canjen lokaci. Wani lokaci shafa ba shine mafita ba.
Lambobin Gaskiya Daga Batches Production
A watan da ya gabata mun shafe tan 3 na LFP ga abokin ciniki a Koriya ta Kudu. Manufa shine 2.8 wt% carbon. Sakamakon batch ya tashi daga 2.65% zuwa 2.95%, wanda ke cikin juriyar mu ± 0.3%. Matsakaicin ƙarfin aiki akan pellet ɗin da aka matse ya kai 8.2 x 10^-3 S/cm.
Don kwatantawa, kayan da ba a rufe su ba sun auna 2.1 x 10^-9 S/cm. Wannan shine kusan sau miliyan 4 haɓakawa a cikin ɗab'i, kodayake kwatanta matsewar pellet conductivity zuwa ɓangarorin ƙwayar cuta ba cikakkiyar dabara ba ce.
Gwajin rayuwa na kewayawa akan sel tsabar tsabar kudi (cajin C / 3, fitarwar C / 3, kewayon 2.5-3.8V) ya nuna ikon riƙewar 91% bayan hawan hawan 1000 a digiri na 25. Manufar abokin ciniki shine 90% don haka ya wuce.
| Nau'in Abu | Abun Carbon | Matsayinmu Na Musamman | Bayanan kula |
|---|---|---|---|
| Katod ɗin LFP | 2-3% | 2.3-2.9% | Mafi na kowa aikace-aikace |
| Anode na LTO | 1-2 kashi cikin ɗari na nauyi | 1.2-1.7% | Kasa da mahimmanci fiye da LFP |
| NCM/NCA | 0.5-1.5% nauyi | 0.8-1.3% | Don kariya ta ƙasa musamman |
| Silicon composite | 5-10% | 6-9% | Bukatar shafa mai sassauƙa |
Matsakaicin da aka nuna shine ainihin abin da muke samu a samarwa, ba makasudin ka'ida ba.

Batutuwa Ingantattun Rubutu Mun gani
Cikakkun ɗaukar hoto shine matsala mafi yawan jama'a, musamman tare da rigar rufi. Za ka ƙare da danda spots a kan barbashi surface wanda halitta gida halin yanzu taro a lokacin hawan keke. Wannan yana nuna sama yayin da ƙarfin ya ɓace bayan zagayowar 200-300.
Mai kauri da yawa yana toshe yaduwar lithium. Muna da tsari guda ɗaya inda rufin ya kasance 25 nm maimakon manufa 10 nm saboda batun kula da zafin jiki. Ƙarfin ƙima ya fi muni muni - sel ba za su iya ɗaukar fitarwar 1C ba tare da raguwar ƙarfin wutar lantarki ba.
Carbon oxidation lokacin ajiya wani batu ne. Ya kamata a adana foda mai rufi a ƙarƙashin yanayin bushe. Muna da abokin ciniki wanda ya adana kayan a cikin ɗakin ajiya mai ɗanɗano har tsawon watanni shida kuma abun cikin carbon ya ragu daga 2.5% zuwa 1.9%. Carbon a hankali yana oxidizes a cikin iska mai danshi.
Kayan aiki da Ƙarfi
Babban tanderun CVD ɗinmu na iya ɗaukar batches 200 kg. Hakanan muna da ƙaramin murhun R&D don batches 5-10 kg lokacin da abokan ciniki ke son gwada sutura akan sabbin kayan. Juyawa don batches R&D yawanci makonni 1-2 ne. Batches samarwa suna ɗaukar makonni 3-4 daga karɓar kayan aiki zuwa jigilar kaya.
Wet shafi line yana da mafi girma kayan aiki, har zuwa 500 kg kowane tsari. Maƙasudin iyakance yawanci shine ƙarfin busasshen feshi maimakon tanderun pyrolysis.
Muna haɓaka ƙarfin shekara mai zuwa tare da sabon tsarin CVD, yakamata ya kasance akan layi ta Q{0}} Ƙarfin manufa shine batches kilo 300 wanda zai taimaka tare da wasu manyan abokan cinikinmu.
Ayyukan Ci gaba
Idan kuna da wani abu wanda zai iya amfana daga shafa amma ba ku da tabbas, za mu iya gudanar da gwaje-gwajen ci gaba. Mafi qarancin yawa yawanci shine gram 200. Za mu gwada yanayin shafi 2-3 daban-daban kuma mu samar da samfurori masu rufi tare da bayanan lantarki daga sel tsabar tsabar kudi.
Farashin ci gaba ya dogara da iyakar gwaji. Ƙimar shafi na asali tare da gwajin ƙwayar ƙwayar cuta yana gudana kusan $ 3500. Idan kuna buƙatar ƙarin gwaji mai faɗi kamar cikakken ginin tantanin halitta ko dogon keken keke na lokaci mai tsawo - zamu iya faɗi wancan daban.
Batu ɗaya da muka ci karo da ita tare da aikin haɓakawa shine cewa sakamakon binciken ba koyaushe yana fassara zuwa sikelin samarwa ba. Mun rufa wani abu a sikelin gram 50 wanda yayi kyau sosai, amma lokacin da muka kai kilogiram 50, daidaiton rufin ya kasance mai muni. Barbashi size rarraba da surface area duka shafi shafi hali da kuma wani lokacin abin da aiki kananan ba ya aiki babban.
Abubuwan Kuɗi
Rufin CVD yana ƙara kusan $2-4 a kowace kilogiram zuwa farashin kayan ya danganta da girman tsari da ƙayyadaddun shafi. Rufin sinadaran rigar shine $ 1.50-2.50 a kowace kg.
Mafi qarancin oda don samar da shafi shine yawanci 50 kg. A ƙasa cewa farashin saitin ya sa ya zama mara inganci. Don adadin haɓaka ƙasa da kilogiram 50 muna cajin kuɗin saiti.
Idan kana siyan precursor abu daga gare mu (wanda ba a rufe foda) kuma yana sa mu sutura, yawanci zamu iya samun farashi mafi kyau fiye da idan kun tura mana kayan ku. Abubuwan dabaru sun fi sauƙi kuma an riga an saita mu tare da masu samar da kayan.
Jirgin da aka rufe yana buƙatar wasu kulawa saboda foda ya fi pyrophoric fiye da kayan da ba a rufe ba. Muna amfani da UN{1}} an yarda da marufi da jigilar kaya ta hanyar jigilar ƙasa kawai. Ba a ba da izinin jigilar jigilar iska don yawancin abubuwan da aka rufa ba{3} saboda haɗarin gobara.
Gwaji da ƙayyadaddun bayanai
Daidaitaccen gwaji muna samarwa tare da kowane tsari:
Abubuwan da ke cikin Carbon ta hanyar nazarin konewa (± 0.1 wt%)
Matsa yawa
Rarraba girman barbashi (D10, D50, D90)
Danshi abun ciki
Hotunan SEM (an bayar akan buƙata)
Akwai ƙarin gwaji:
Ma'auni na ɗabi'a akan pellet ɗin da aka danna
BET surface area
XRD don tsarin crystal
TEM giciye{0}} sassan don tabbatar da kauri
ICP{0}MS don nazarin ƙazanta
Gwajin cell Coin (aikin hawan keke, iyawar ƙimar, impedance)
Yawancin abokan ciniki kawai suna son ainihin gwaji da ma'aunin aiki. Cikakken halayyar yana ƙara kusan mako guda zuwa lokacin juyawa da ƙarin farashi.

Abin da Ba Mu Yi ba
Ba ma suturar zanen wutan lantarki. An tsara kayan aikin mu don suturar foda. Idan kuna buƙatar shafa akan riga-kafi{2}}waɗanda aka ƙera na'urorin lantarki wannan tsari ne na daban gaba ɗaya.
Har ila yau, ba ma sarrafa kayan da ke da matsalolin tsaro masu tsanani. Babu foda na ƙarfe na lithium, babu iskar daɗaɗɗa{1} Daidaitaccen kayan baturi yana da kyau amma idan kayanka ba da jimawa ba ya ƙone cikin iska ba za mu iya aiki da shi ba.
Ultra{0}Maɗaukaki mai tsabta (jinin semiconductor) ba shine abin da muka mayar da hankali ba. An saita mu don kayan baturi wanda ke nufin tsabta mai kyau amma ba matakin ɗaki mai tsabta ba. Idan kuna buƙatar kulawar gurɓataccen ƙwayar cuta ta ppm - kuna buƙatar wani nau'in makaman daban.
Misalan Abokin Ciniki
Wani kamfanin batir a Michigan ya aiko mana da siliki - graphite composite anode abu. Suna ganin iya aiki yana dushewa bayan zagayowar 150. Mun lullube shi da tsarin carbon ɗin mu mai sassauƙa kuma sun sami rayuwar zagayowar har zuwa zagayowar 600. Farashin kayan ya karu da $3.50/kg amma haɓaka aikin ya ba da hujjar aikace-aikacen su.
Wani aikin ya haɗa da shafa NCM811 don abokin ciniki na kera motoci na Turai. Sun damu game da faɗuwar iya aiki a babban ƙarfin lantarki (yankewar 4.3V). Madaidaicin NCM811 ya nuna asarar iya aiki 15% bayan zagayowar 500. Tare da 1 wt% carbon shafi tare da wasu jiyya na saman mun sami wannan ƙasa zuwa asarar iya aiki 8%. Rufin ba shine kawai dalilin ba {11} kuma sun inganta electrolyte ɗin su - amma ya taimaka.
Mun yi aiki tare da ƙungiyar bincike suna haɓaka sabon abun da ke ciki na cathode (lithium{0}} bambancin NCM mai arziƙi). Kayan yana da iya aiki mai kyau amma mugun iyawar ƙimar. Bayan shafa tare da 2% carbon ƙarfin fitarwa a 1C ya inganta daga 140 mAh/g zuwa 168 mAh/g. Ƙarfafawa ita ce ƙayyadaddun abu ga abin.
Wani lokaci shafa baya magance matsalar. Muna da abokin ciniki tare da saurin iya aiki a cikin ƙwayoyin su kuma suna tunanin sutura zai gyara shi. Bayan bincike mun gano cewa sun lalace saboda lithium plating akan anode yayin caji mai sauri. Rufe cathode ba zai taimaka da hakan ba. Mun ba da shawarar su duba ka'idar cajin su maimakon.
Albarkatun Fasaha
Mun buga wasu takardu akan murfin carbon idan kuna son ƙarin cikakkun bayanai kan kimiyya. Yawancin suna bayan bangon biyan kuɗi amma za mu iya aika PDFs idan kun tuntube mu.
Idan kuna aiki tare da kayan aikin phosphate na lithium kuma kuna son fahimtar ɓangaren sinadarai na baturi, wannan labarin akan [lithium ion phosphate baturi] ya rufe abubuwan yau da kullun da kyau. Fahimtar sinadarai na baturi yana taimakawa bayyana dalilin da yasa sutura ke yin irin wannan bambanci ga LFP musamman.